Spots appear locally on polished cement screed (waxed concrete)

Solutions

Spots appear locally on polished cement screed (waxed concrete)

Technical Support +30 2103633512 Mon - Fri: 9:00 - 17:00

POTENTIAL CAUSES OF THE PROBLEM

  • Possible entrapped moisture content on the substrate
  • Varnish was applied too early, entrapping moisture in the substrate
  • Bad choice of varnish (water varnish chosen in wet areas instead of polyurethane varnish)
  • Bad application of varnish

Product Categories

Steps

STEP 1 Surface rubbing with an electric sander to remove varnish.
STEP 2 Leave the surface as long as it is needed for moisture to evaporate.
STEP 3 Apply GLX 292 FLEX PRIM.
STEP 4 Apply DECOR PU VARNISH (mat or gloss) in two coats. The second coating is applied after the first one is dry. In case of upcoming moisture, remove polished cement screed and proceed to waterproofing substrate with DSF 353 SUPER ELASTIC before application of DECOR.

Products Used

DECOR PU VARNISH
Πολυουρεθανικό βερνίκι 2 συστατικών
Cement based SUPER ELASTIC DSF 353
Flexible 2-component, cement based, brushable sealing slurry
MICROCEMENT DECOR GLX 292 FLEX PRIM