Solutions
Cracks on masonry build with AAC blocks
Solutions
Cracks on masonry build with AAC blocks
POTENTIAL CAUSES OF THE PROBLEM
- Application of final coat plaster directly on AAC blocks.
- Application was not made with the proper tools
Product Categories
SOLUTION
STEP 1
Clean thoroughly with a brush, the surface from dust and loose particles.
STEP 2
Start repairing the cracked surface with the fast-setting repairing mortar REPIFIX WRM 520.
STEP 3
Prime the surface with deep penetration primer, GLX 292 FLEX PRIM.
STEP 4
Apply the first layer of fiber-reinforced base coat, THC 410.
STEP 5
As long as THC 410 is still wet, firmly CLIMAPLUS fiberglass mesh (160 g/m²).
STEP 6
Then, apply a second layer of fiber-reinforced, base coat, THC 410, in order to completely cover the mesh.
STEP 7
Prime the surface of application with the colored acrylic primer GLX 494 PRIM.
STEP 8
Apply the organic acrylic-based top coating DEC 428, at the color tone of our selection from the CLIMAPLUS fan deck.
STEP 9
Apply the organic acrylic-based top coating DEC 428, at the color tone of our selection from the CLIMAPLUS fan deck.
STEP 10
ATTENTION: If the application is in a seaside area or an area with high moisture content, THRAKON suggests the application of our silicone system. In such a case, proceed to the following steps:
a) Prime the surface with the colored silicone-based primer GLX 498 CLIMASIL PRIMER.
b) Application of organic silicone-based top coating DEC 438, in the color tone of our selection from the CLIMAPLUS fan deck.
Products Used