POTENTIAL CAUSES OF THE PROBLEM

No application of diagonal fiberglass mesh for reinforcing plaster at the corners of openings (windows, doors).

Product Categories

SOLUTION

STEP 1 Widening of the crack at 3cm depth.
STEP 2 Level the surface with STATUS Acrylic Putty.
STEP 3 Apply one layer of CLIMAFLEX THC 410.
STEP 4 Apply fiberglass mesh before CLIMAFLEX THC 410 dries, in the opposite direction of the opening.
STEP 5 Apply REPIFIX FAST WRM 550.