POTENTIAL CAUSES OF THE PROBLEM

Problem: insufficient adhesion, resulting from:

a) It probably rained shortly after the paint was applied

b) Possible moisture from the substrate

c) Apply paint in prohibitive weather conditions (high temperatures)

Product Categories

SOLUTION

STEP 1 Using sandpaper, remove all loose material, then thoroughly wipe the surface clean.
STEP 2 Fill where required with STATUS 100 % acrylic putty.
STEP 3 Prime with Primer STATUS DUR.
STEP 4 Apply two coats of STATUS ALL WEATHER.

Products Used

PAINTS STATUS DUR
Waterproofing solvent-based acrylic primer
Acrylic Paints / Tinted Bases STATUS ALL WEATHER