Solutions
Detachment of plasters
Solutions
Detachment of plasters
POTENTIAL CAUSES OF THE PROBLEM
- Strain from the weather: Moisture can corrode mud over time.
- The application was performed at a high temperature, resulting in poor adhesion between plaster layers.
- Inadequate material selection.
- Ingress of moisture into the substrate due to cracks.
- Application under unsuitable conditions (temperature > 35 °C).
Product Categories
SOLUTION
STEP 1
Firstly, all crumbling parts of plaster are removed with a spatula, and the surface is cleaned off with a brush.
STEP 2
Prime the surface with the deep penetration primer GLX 292 FLEX PRIM.
STEP 3
Application of REPIFIX RAPID WRM 520, which is fast-setting, on the surface of application. Wait 20 minutes for it to dry.
STEP 4
Application of REPIFIX TOP WRM 483 is a cementitious putty, ideal for applications on concrete.
STEP 5
As soon as REPIFIX TOP WRM 483 dries, proceed to the rubbing of the surface.
STEP 6
Application of the deep penetration primer, GLX 292 FLEX PRIMER.
STEP 7
Paint the surface with STATUS ALL WEATHER in two coats.
Products Used