POTENTIAL CAUSES OF THE PROBLEM

  • The paint was subjected to intense sunlight before it had the chance to dry.
  • Significant contraction of the substrate occurred, which the paint could not accommodate as it lacked resilience.

Product Categories

SOLUTION

STEP 1 Rub the surface to remove any loose material.
STEP 2 Clean the surface thoroughly.
STEP 3 Prime the surface using a high-penetration acrylic primer, such as GLX 292 FLEX PRIM or STATUS DUR.
STEP 4 Apply a sealing elastomeric paint, specifically STATUS ALL WEATHER, to the surface.

Products Used

MICROCEMENT DECOR GLX 292 FLEX PRIM
High penetration micronized acrylic primer
PAINTS STATUS DUR
Waterproofing solvent-based acrylic primer
Acrylic Paints / Tinted Bases STATUS ALL WEATHER
Elastomeric Waterproof Facade Paint