Light acrylic putty
POTENTIAL CAUSES OF THE PROBLEM
No application of diagonal fi berglass mesh, for reinforcing plaster at the corners of openings (windows, doors).
SOLUTION
1: Widening of crack at 3cm depth
2: Levelling of surface with STATUS ONE COVER
3: Application one layer of THC 410C
4: Application of fi berglass mesh, before THC 410C gets dried (on the opposite direction of the opening)
5: Application of repairing plaster WRM 550
Light acrylic putty
Fast setting repairing plaster
Coarse-grained, flexible, fiber reinforced, adhesive – plaster