Cracks > 1cm
What do we need?
Cracks >1cm often appear in masonry filling are a danger to their statics.
How do we do it?
The repair of the cracks of the walls is necessary by using specialized materials that provide a permanent long-term solution.
Products used
WRM 520
WRM 550
Fiberglass for wall reinforcement (223g/m2)
Step by step
- Start by widening the crack by 15-20cm on each side and the opening decoupling with a sharp tool (V shape).
- Clean surface from dust and loose particles. Spray the area of the application and apply fast setting repairing mortar WRM 520.
- After 20-30 min is the restoration of crumbled and detached plaster with fast setting repair plaster WRM 550, arming the application thickness using THRAKON repairing fibreglass mesh (223g/m2). The fiberglass gets 2/3 of the total thickness of the repair plaster WRM 550.
- Next day is the restoration of crumbled and detached plaster with fast setting repairing plaster WRM 550.
Product Categories :
Repairing mortars
Share